1. Rough grinding of surface: After preliminary forming of carbon fiber auto parts, rough grinding of sandpaper or grinding wheel is needed to ensure smooth surface;
2. Washing: excess carbon powder particles remain on the surface of carbon fiber auto parts after coarse grinding, which need to be washed;
3, dry: with a good absorbent cloth to dry carbon fiber auto parts surface water stains;
4, baking: through autoclave or vacuum autoclave baking molding;
5, painting: according to customer needs for surface painting, primer, color paint, surface transparent paint, etc.
6, two drying: after the completion of the painting need to dry again, multiple painting, you need to dry several times;
7, surface grinding: carbon fiber auto parts surface paint is uneven or limited, need to go through fine grinding to achieve smooth surface;